Producing Load Bearing Block Using LECA as Partial Replacement of Coarse Aggregate
The ability to produce load-bearing masonry units adopting ACI 211.1 mix design using (1:3.2:2.5) as (cement: fine aggregate: coarse aggregate) with slump range (25-50mm) which can conform (dimension, absorption, and compressive strength) within IQS 1077/1987 requirements type A was our main goal of the study.The ability to use low cement content (